Butadiene Rubber

The BR family of polybutadiene rubber helps optimize tire compositions, improving grip, fuel economy, and overall lifetime. They provide a great balance between processability and performance.

Buna® CB 1203 Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 43 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® CB 1220 AO Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 40 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® CB 1221 Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® CB 22 Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® CB 24 Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® CB 25 Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® Nd 22 EZ Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® Nd 24 EZ Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %

Emulsion Styrene Butadiene Rubber

E-SBR is predominantly used for the production of car tires, light truck tires and truck tire retread compounds. It presents good mechanical properties, abrasion, and tear resistance.

Buna® SE 1500 Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Buna® SE 1502 H Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Buna® SE 1502 L Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775

Functionalized & Standard S-SBR and Block Co-Polymers

The tire industry is the main market segment for S-SBR. S-SBR offers improved wet grip and reduced rolling resistance — which translate to greater safety and better fuel economy.

Buna® SL 4518-4 Standard S-SBR (Buna SL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 18 wt % ASTM D 5775
Oil Content 27,3 wt % ASTM D 5774
Buna® SL 4525-0 Standard S-SBR (Buna SL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 25 wt % ASTM D 5775
Buna® SL 7518-4 Standard S-SBR (Buna SL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 75 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 18 wt % Internal Method
Oil Content 13 wt % ASTM D 5774