Regular Butyl & Halogenated Butyl Rubber

Butyl rubber (IIR) is a synthetic rubber, a copolymer of isobutylene with isoprene. Providing excellent air retention, it is widely used for tire inner liners among other applications.

X_Butyl® BB 2030 Bromobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 32 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Bromine Content 1,80 wt % Internal Method
Antioxidant non-staining > 0,03 wt % Internal Method
Ash Content < 0,7 wt % ISO 247 / ASTM D 5667
Volatile Content < 0,7 wt % ISO 248 / ASTM D 5668
X_Butyl® BB 2040 Bromobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 39 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Bromine Content 1,80 wt % Internal Method
Antioxidant non-staining > 0,03 wt % Internal Method
Ash Content ≤ 0,7 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,7 wt % ISO 248 / ASTM D 5668
X_Butyl® BB X2 Bromobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 46 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Bromine Content 1,80 wt % Internal Method
Antioxidant non-staining > 0,03 wt % Internal Method
Ash Content ≤ 0,7 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,7 wt % ISO 248 / ASTM D 5668
X_Butyl® CB 1240 Chlorobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 38 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Chlorine Content 1,25 wt % Internal Method
Antioxidant non-staining > 0,03 wt % Internal Method
Ash Content ≤ 0,5 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,5 wt % ISO 248 / ASTM D 5668
X_Butyl® RB 101-3 Regular Butyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 51 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Unsaturation 1,75 %(Mol) (*)
Ash Content ≤ 0,3 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 1 wt % ISO 248 / ASTM D 5668
X_Butyl® RB 301 Regular Butyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 51 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Unsaturation 1,85 %(Mol) (*)
Antioxidant non-staining > 0,03 wt % Internal Method
Ash Content ≤ 0,3 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,3 wt % ISO 248 / ASTM D 5668
X_Butyl® RB 402 Regular Butyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 33 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Unsaturation 2,25 %(Mol) (*)
Antioxidant non-staining > 0,03 wt % Internal Method
Ash Content ≤ 0,3 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,3 wt % ISO 248 / ASTM D 5668

BUTADIENE RUBBERS (BR)

The BR family of polybutadiene rubber helps optimize tire compositions, improving grip, fuel economy, and overall lifetime. They provide a great balance between processability and performance.

Buna® CB 22 Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Density 0,91 g/cm3 ASTM D 297

EMULSION-STYRENE BUTADIENE RUBBERS (E-SBR)

E-SBR is predominantly used for the production of car tires, light truck tires and truck tire retread compounds. It presents good mechanical properties, abrasion, and tear resistance.

Buna® SE 1502 H Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Density 0,94 g/cm3 ASTM D 297

Hydrogenated Nitrile Butadiene Rubber

ARLANXEO's HNBR products, summarized under the Therban® brand, offer excellent properties wherever high temperature and fluid resistance is needed. The polarity of HNBR is directly influenced by the ACN content. Higher ACN increases the polymer's polarity and, therefore, resistance in non-polar...

Therban® 3406 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Density 0,95 g/cm3 Internal Method
Therban® 3406 SF Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Density 0,95 g/cm3 Internal Method
Therban® 3407 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Density 0,95 g/cm3 Internal Method
Therban® 3446 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 61 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 3,95 % IR Spectroscopy
Density 0,95 g/cm3 Internal Method
Therban® 3467 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 68 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 5,5 % IR Spectroscopy
Density 0,95 g/cm3 Internal Method
Therban® 3496 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 18,0 % IR Spectroscopy
Density 0,96 g/cm3 Internal Method
Therban® 3607 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 66 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Density 0,95 g/cm3 Internal Method
Therban® 3627 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 66 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 2,0 % IR Spectroscopy
Density 0,96 g/cm3 Internal Method
Therban® 3629 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 87 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 2,0 % IR Spectroscopy
Density 0,96 g/cm3 Internal Method
Therban® 3907 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 39,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Density 0,96 g/cm3 Internal Method