Ethylene Propylene Diene Rubber

EPDM is typically used in outdoor applications and at elevated temperatures of up to 150 °C. It's used in both automotive and industrial applications such as automotive sealing systems, coolant hoses, windshield wipers, oil additives, roof sheeting, window gaskets, conveyor belts, as well as wire...

Keltan® 0500R Downsheared
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 11 g/10mi ASTM D 1238
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 49 wt % ASTM D 3900
Density 0,86 g/cm3 Internal Method
Keltan® 1500R Downsheared
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 2,55 g/10mi ASTM D 1238
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 49 wt % ASTM D 3900
Density 0,86 g/cm3 Internal Method
Keltan® 1519R Downsheared
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 4,5 g/10mi ASTM D 1238
Molecular Weight Distribution Narrow Internal Method
Maleic Anhydride Content 1,9 wt % Internal Method
Ethylene Content 49 wt % ASTM D 3900
Keltan® 3050 Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 51 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 49 wt % ASTM D 3900
Density 0,86 g/cm3 Internal Method

Ethylene Vinyl Acetate Rubber

ARLANXEO’s EVM rubbers are sold under the tradenames Baymod® L, Levamelt® and Levapren®. EVM rubbers are produced by copolymerization of ethylene and vinyl acetate. Our ethylene-vinyl acetate copolymers are used as synthetic rubbers, or as modifiers in thermoplastics, specifically PVC. The main...

Levapren® 500 General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 50 wt % Internal Method LP 015
Density 1,00 g/cm3 Internal Method

Hydrogenated Nitrile Butadiene Rubber

ARLANXEO's HNBR products, summarized under the Therban® brand, offer excellent properties wherever high temperature and fluid resistance is needed. The polarity of HNBR is directly influenced by the ACN content. Higher ACN increases the polymer's polarity and, therefore, resistance in non-polar...

Therban® 3407 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Density 0,95 g/cm3 Internal Method