Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,98 g/cm3 |
Internal Method |
|
|
Particle Size |
≤ 0,7 mm |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
70 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,98 g/cm3 |
Internal Method |
|
|
Particle Size |
0,7 mm |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
55 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
1,01 g/cm3 |
Internal Method |
|
|
Particle Size |
0,3 mm |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
55 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
1,01 g/cm3 |
Internal Method |
|
|
Particle Size |
0,3 mm |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
115 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
38,0 wt % |
ISO 24698 |
|
|
Density |
1,01 g/cm3 |
Internal Method |
|
|
Particle Size |
0,08 mm |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
48 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
27,5 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
65 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
28,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
110 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
30 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
30 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
44 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
70 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
50 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
43,5 wt % |
ISO 24698 |
|
|
Density |
1,00 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
55 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
48,5 wt % |
ISO 24698 |
|
|
Density |
1,00 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
75 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
48,5 wt % |
ISO 24698 |
|
|
Density |
1,00 g/cm3 |
Internal Method |
|
|
|
Krynac® M 3340 F
Plasticizer Extended
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
33 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33 wt % |
ISO 24698 |
|
|
Density |
0,98 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
78 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Density |
1,06 g/cm3 |
Internal Method |
|
|
|
Krynac® X 146
Carboxylated
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
32,5 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
Krynac® X 160
Carboxylated
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
58 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
32,5 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
Krynac® X 740
Carboxylated
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
38 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
26,5 wt % |
ISO 24698 |
|
|
Density |
0,99 g/cm3 |
Internal Method |
|
|
|
Krynac® X 750
Carboxylated
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
47 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
27,0 wt % |
ISO 24698 |
|
|
Density |
0,99 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
47 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Chlorine Content |
< 0,1 wt % |
Internal Method |
|
|
Acrylonitrile Content |
27,0 wt % |
ISO 24698 |
|
|
Density |
0,99 g/cm3 |
Internal Method |
|
|
|
Krynac® XL 3355
Pre-Crosslinked
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
55 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
1,00 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
75 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
33,0 wt % |
ISO 24698 |
|
|
Density |
1,00 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
18,0 wt % |
ISO 24698 |
|
|
Density |
0,93 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
52 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
22,0 wt % |
ISO 24698 |
|
|
Density |
0,94 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
120 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
28,0 wt % |
ISO 24698 |
|
|
Density |
0,96 g/cm3 |
Internal Method |
|
|
|
Perbunan® 2831 F
Fast Cure Clean
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
30 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
28,6 wt % |
ISO 24698 |
|
|
Density |
0,96 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
28,0 wt % |
ISO 24698 |
|
|
Density |
0,96 g/cm3 |
Internal Method |
|
|
|
Perbunan® 2846 F
Fast Cure Clean
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
42 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
28,6 wt % |
ISO 24698 |
|
|
Density |
0,96 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
70 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
28,0 wt % |
ISO 24698 |
|
|
Density |
0,96 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
95 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
28,0 wt % |
ISO 24698 |
|
|
Density |
0,96 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
32 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
34,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
Perbunan® 3436 F
Fast Cure Clean
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
34 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
34,7 wt % |
ISO 24698 |
|
|
Density |
0,98 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
34,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
Perbunan® 3446 F
Fast Cure Clean
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
42 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
34,7 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
70 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
34,0 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
Perbunan® 3481 F
Fast Cure Clean
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
78 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
34,7 wt % |
ISO 24698 |
|
|
Density |
0,97 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
45 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
39,0 wt % |
ISO 24698 |
|
|
Density |
0,99 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
65 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
39,0 wt % |
ISO 24698 |
|
|
Density |
0,99 g/cm3 |
Internal Method |
|
|
|
|
Property |
Nominal Value |
Test Method |
Condition |
Temperature |
Mooney Viscosity |
55 MU |
ISO 289 / ASTM D 1646 |
ML (1+4) |
100 °C |
Acrylonitrile Content |
44,0 wt % |
ISO 24698 |
|
|
Density |
1,01 g/cm3 |
Internal Method |
|
|
|